SAE Technical Standards Board Rules provide that: “This report is published by SAE to advance the state of technical and engineering sciences. The use of this report is entirelyvoluntary, and its applicability and suitability for any particular use, including any patent infringement arising therefrom, is the sole responsibility of the user.”

SAE reviews each technical report at least every five years at which time it may be reaffirmed, revised, or cancelled. SAE invites your written comments and suggestions.

QUESTIONS REGARDING THIS DOCUMENT: (412) 772-8512 FAX: (412) 776-0243

TO PLACE A DOCUMENT ORDER; (412) 776-4970 FAX: (412) 776-0790

Copyright 1985 Society of Automotive Engineers, Inc.All rights reserved.

Printed in U.S.A.

SAE J1326 Revised FEB855.5.1ProcedureImmerse the test specimen in either freshly boiled distilled water or deionized water from an ion-exchangedevice at room temperature with occasional agitation to insure thorough wetting out (approximately 15 mingenerally required).Remove the specimen and pass through the wringer to remove excess liquid when the wet mass is more thanthree times the dry mass. Whenever possible, the wet mass of the specimen will be 2.5 - 3 times its dry mass.Place the specimen between glass or plastic plates and insert in the specimen unit of the perspiration tester.Adjust the perspiration tester to produce a pressure of 14 kPa on the specimen.Place the loaded specimen unit in an oven at 38 ± 1°C so that the plates are in a vertical position and heat for18 h. Remove the specimen from the unit and complete drying by hanging in air at room temperature. Do notpress dry.Report—Classify the staining:CLASS 5 - neglible or no stainingCLASS 4 - staining equivalent to Row 4 on the AATCC scaleCLASS 3 - staining equivalent to Row 3 on the AATCC scaleCLASS 2 - staining equivalent to Row 2 on the AATCC scaleCLASS 1 - staining equivalent to Row 1 on the AATCC scale7.7.1NotesMarginal Indicia—The change bar (I) located in the left margin is for the convenience of the user in locatingareas where technical revisions have been made to the previous issue of the report. An (R) symbol to the left ofthe document titles indicates a complete revision of the report.5.25.35.46.PREPARED BY THE SAE NONMETALLIC MATERIALS COMMITTEE-2-SAE J1326 Revised FEB85Rationale—Not applicable.Relationship of SAE Standard to ISO Standard—Not applicable.Application—This procedure describes a method of measuring the resistance to wet color transfer of dyed,printed, or otherwise colored textile yarns and composites thereof.Reference Section—There are no referenced publications specified herein.Developed by the SAE Nonmetallics Materials Committee